This article considers a technological method of influencing the thermomechanical state (with reduced plasticity) of the crystallizing metal of a welded joint when welding metals with accompanying preheating. It is noted that the effect of accompanying preheating is manifested when the preheating tool is optimally positioned relative to the welding arc. Methane, propane-butane gas can be used for plates thicker than 10 mm, and the electric arc without melting the base metal up to 10 mm thick. The preheating tool has a speed adequate to the welding speed.

  • Ссылка в интернете
  • DOI
  • Дата создание в систему UzSCI 14-06-2024
  • Количество прочтений 76
  • Дата публикации 01-04-2024
  • Язык статьиIngliz
  • Страницы7-9
English

This article considers a technological method of influencing the thermomechanical state (with reduced plasticity) of the crystallizing metal of a welded joint when welding metals with accompanying preheating. It is noted that the effect of accompanying preheating is manifested when the preheating tool is optimally positioned relative to the welding arc. Methane, propane-butane gas can be used for plates thicker than 10 mm, and the electric arc without melting the base metal up to 10 mm thick. The preheating tool has a speed adequate to the welding speed.

Имя автора Должность Наименование организации
1 TALIPOV M.M. PhD Tashkent State Transport University
2 TALIPOVA G.D. Senior Teacher Tashkent Railway College
Название ссылки
1 Gelman A.S., Melbard S.K. “Submerged arc welding with high-temperature heating in the welding zone.” “Welding production” No. 3, 1960
2 Dyatlov V.I., Sidoruk V.S. Influence of technological conditions on the formation of hot longitudinal cracks. Automatic welding No. 3, 1961
3 Gura R.M. “Study of welded joints of pipes made by heating from austenitic steels EP-17, EP-18I and EI 695RG.” Collection “Metal in modern power plants”, Moscow, Publishing House “Energia”, 1965
4 Prokhorov I.I., Prokhorov Nik I., Magerramov A.G. “Study of the influence of heating on the processes of development of internal stresses and deformation during welding.” “Physics and chemistry of materials processing” No. 6, 1972
5 Dietrich E. Preheating temperatures when welding high-strength structural steels. "Schweiss Technic" No. 3, 1968
6 Herold Hornt. Checking preheating temperatures during welding using time-temperature-transformation diagrams. "Schweiss Technic" No. 1, 1972
7 Kihara N. Study on preheating temperature welds of high-stranght Steel structure. "Transactions of the Japan Welding Society", 1970
8 Fomin V.V., Yushchenko K.A., Kakhovsky M.I., Ponizovtsev A.M. Welding of stainless steels with a consumable electrode, additionally heated by alternating and direct current. Information letter No. 58, 1968 Institute of Electric Welding named after E.O. Paton Academy of Sciences USSK, Kyiv
9 Kakhovsky N.I., Yushchenko K.A., Ponizovtsev A.M., Fomin V.V. Gas-electric welding with a consumable heated electrode. Information letter Institute of Electric Welding named after E.O. Paton Academy of Sciences USSK, Kyiv. 1971
10 Kasimov A.M., Balandin S.L. The influence of accompanying heating on crack formation in a weld during welding. TADI Bulletin, 2015
11 Kasimov A. M. Experience in welding fixed joints of pipes made of steel 15X1M1F with heating. Automatic welding, 1975
В ожидании